vol.32 número1Cambios en incisivos y su relación con el punto A y el ángulo nasolabial en pacientes Clase II división 2 tratados con y sin extracciones en el Centro Dental Docente UPCH.Porphyromonas gingivalis en fluido crevicular de pacientes diabéticos tipo 2. índice de autoresíndice de materiabúsqueda de artículos
Home Pagelista alfabética de revistas  

Servicios Personalizados

Revista

Articulo

Indicadores

  • No hay articulos citadosCitado por SciELO

Links relacionados

  • No hay articulos similaresSimilares en SciELO

Compartir


Revista Estomatológica Herediana

versión impresa ISSN 1019-4355

Resumen

VASQUEZ-CASTRO, Eva et al. Evaluation of the exposure time of a Bulk-Fill resin in deep preparations. Rev. Estomatol. Herediana [online]. 2022, vol.32, n.1, pp.30-35.  Epub 22-Abr-2022. ISSN 1019-4355.  http://dx.doi.org/10.20453/reh.v32i1.4180.

Background:

Bulk-fill composite resins (BF) are used in posterior restorations with extensive and deep preparations. One of the most outstanding benefits is that it can be used in increments of 4 to 5 mm, reducing clinical working time. However, in teeth with root canal treatment, these preparations could be deeper.

Objectives:

To determine the photoactivation time necessary to polymerize a Bulk-Fill resin located in deep areas.

Material and Methods:

In the present experimental in vitro study, specimens of Filtek One Bulk Fill composite resin (3M ESPE, St. Paul, USA) of 5x5x5 mm color A2 photoactivated at a distance/time of 0 mm/10 s, 0 mm/20 s, 3 mm/10 s, 3 mm/20 s, 3 mm/30 s and 3 mm/40 s (n=5) were fabricated. Surface microhardness was recorded on the surface and at the base of each specimen.

Results:

The highest microhardness value was recorded in group BF 0 mm/20 s and BF 3 mm/40 s (p<0.05), followed by groups BF 3 mm/20 s and BF 3 mm/30 s (p>0.05). The lowest microhardness values were found in the BF 0 mm/10 s and BF 3 mm/10 s groups.

Conclusion:

It takes 40 s of photoactivation to polymerize a Bulk-Fill resin located in deep areas, when the lamp is 3 mm away from the resin surface.

Palabras clave : Hardness; time; composite resins; polymerization.